Seal Material Selector
Compare common seal-material families using the operating environment. This is a screening aid—not a substitute for the exact compound data sheet and seal-profile design limits.
Material families at a glance
The selector ranks four common families from your inputs. The table below adds the families it deliberately routes elsewhere, and the cautions that most often change a decision. It describes broad families; individual compounds differ, so the compound data sheet and the seal maker’s limits for the exact profile always take priority.
| Family | Typical role | Why it is chosen | Check before use |
|---|---|---|---|
| PU / HPU (thermoplastic polyurethane) | Dynamic rod and piston seals, U-cups, wipers | High abrasion and extrusion resistance in mineral-oil service | Standard grades can hydrolyse in water-based fluids and hot water; upper temperature is limited for many grades. HPU is a supplier designation, not one compound. |
| NBR (nitrile) | O-rings, static seals, energizers, some dynamic seals | Widely used with mineral hydraulic oils; economical and available in many sizes | Hardens with sustained heat; not a first choice for phosphate-ester fluids; check the exact compound for other fluids. |
| FKM (fluoroelastomer) | Static seals and energizers in hot or chemically demanding service | Higher temperature capability and broad chemical resistance | Low-temperature flexibility varies by grade; conventional FKM is not automatically suitable for phosphate esters. |
| PTFE (filled), elastomer-energized | Low-friction step and slipper seals for rods and pistons | Low friction and low stick-slip tendency; broad chemical and temperature range | Needs an energizer whose own material must suit the fluid; often needs sizing after installation; filler affects the counter-surface. |
| EPDM | Phosphate-ester (e.g. Skydrol-type) systems when approved | Used where phosphate-ester compatibility is required | Not suitable for mineral hydraulic oil. Use only with the fluid maker’s or seal maker’s approval. |
| POM (acetal) and filled guide materials | Guide rings, back-up rings, anti-extrusion elements | Rigid support at the extrusion gap and side-load bearing | Not a primary flexible sealing element. |
How the screen scores
Each family starts from a fixed base score that is raised or lowered by fluid, duty, temperature, pressure, speed and contamination. Temperatures outside the broad range used here (about −30 to 100 °C for PU and NBR, about −15 to 200 °C for FKM and about −50 to 200 °C for PTFE) are flagged for compound-specific verification.
Why a ranking is not a specification
Seal life depends on the profile, the extrusion gap, the surface finish and the energizer as much as on the base polymer. Use the ranking to decide which data sheets to request, not which part to order.